Stainless steel solutions
Raw materials technical specificationsТехнически характеристики на материалитеТехнические характеристики
StandartsСтандартиСтандарты
USA - ASTM / AISI 304 304L 310 316 316L 321
GOST 08Ch18N10 03Ch18N11 20Ch23N18 08Ch16N11M3 03Ch17N14M3 08Ch18N10T
BRD - W.NR. / DIN 1.4301 1.4306 1.4845(1.4841 1.4401 1.4404(1.4435 1.4541
IT - UNI X5CrNi1810 X2CrNi1911 X12CrNi2521 X5CrNiMo17122 X2CrNiMo17132 X6CrNiTi1810
FR - AFNOR Z7CN18-09 Z3CN19-121 Z7CND17-12-02 Z3CND18-12-02 Z6CNT18-10 Z6CNDT17-12
Chemical composition - %Химически състав - %Химический состав - %
C (max) 0.08 0.03 0.25 0.08 0.03 0.08
Si (max) 1 1 1.5 1 1 1
Mn (max) 2 2 2 2 2 2
P (max) 0.045 0.045 0.045 0.045 0.045 0.045
S (max) 0.03 0.03 0.03 0.03 0.03 0.03
Cr 17.0-20.0 18.0-20.0 24.0-26.0 16.0-18.5 16.0-18.5 17.0-19.0
Ni 8.0-10.5 8.0-12.5 19.0-22.5 10.0-14.0 10.0-14.0 9.0-12.0
OtherДругиДругие - - - Mo2.00-3.00 Mo2.00-3.00 Ti – 0.3
Physical and mechanical characteristicsФизически и механически характеристикиФизические и механические характеристики
Tensile strenght, Rm MPaЯкост на опън, Rm MPaЯкость натягив.,Rm MPa 500-700 460-680 500-700 510-710 490-690 500-730
Yield strenght, Re/min/ MpaГран. на провл.,Re/min/ MpaГран. проволоч., Re/min/ Mpa 195 180 210 205 190 200
Elongation, min % A5Удължение, min % A5Удолжение, min % A5 45 45 35 40 40 40
Thermal expansion,10-6К-1Темп. Разширение,10-6К-1Темп. разширение при t- С° 16.0/100 С° 19.0/800 С° 16.0/100 С° 19.0/800 С° 17.0/400 С° 19.0/1000 С° 16.5/100 С° 19.5/800 С° 16.5/100 С° 19.5/800 С° 16.0/100 С° 19.0/800 С°
Hardness, HB 30Твърдост, HB 30Твэрдость,HB 30 130-180 120-180 192 130-180 120-180 130-190
Conductivity, W.mm2/mЕл.проводимост, W.mm2/mEl.Ел.проводимость, W.mm2/m 0.73 0.73 0.85 0.75 0.75 0.73
Heat conductivity, W/K.mТоплопроводимост, W/K.mТеплопроводимость, W/K.m 15 15 14 15 15 15
PermanenceМагнитна проводимостМагнитная проводимость 1003 1003 1010 1003 1003 1002